FEATURES OF THE PHYSICAL AND MECHANICAL CHARACTERISTICS OF DIAMOND POWDER, AC20 GRADE, GRAIN 100/80, AND THE PRODUCTS OF ITS FLOTATION SEPARATION

  • N.O. Oliinyk Інститут надтвердих матеріалів ім. В. Бакуля
  • G.D. Ilnitska Інститут надтвердих матеріалів ім. В. Бакуля
  • G.A. Petasyuk Інститут надтвердих матеріалів ім. В. Бакуля
  • G.A. Bazaliy Інститут надтвердих матеріалів ім. В. Бакуля
Keywords: synthetic diamond grinding powder, flotation, strength, morphometric characteristics

Abstract

The physico-mechanical characteristics of AC20 diamond powder with a grain size of 100/80 and the products of its flotation separation were studied. Separation was carried out in one stage. The work uses well-known methods of researching synthetic diamond powders. Static strength was investigated using the DA-2 device, morphometric characteristics were investigated using the DiaInspect. OSM device. It was established that the use of flotation separation of AC20 diamond powder with a grain size of 100/80 allows to obtain diamond powder with an increased strength index under static compression by 23.8%, increased uniformity in strength by 25.0%, a significantly reduced proportion of impurities and inclusions, and morphometric characteristics close to the original powder.

Published
2023-10-07
Section
Статті